Phone
Phone

TS-series foam uses ultra-low compression force to deform before the cells do, turning cyclical swelling into elastic foam compression instead of hard cell-to-cell pressure. Just ~30 kPa at 25% compression, density from 230 kg/m³, and compression set under 5% (50%, 100°C, 22 h) give flexible, long-life support between cells and across module beams. UL 94 V-0 certified (File No. E499089) and stable from −55°C to 200°C, it also seals against dust and moisture across EV and ESS packs. See our silicone foam selection guide for key checkpoints.
Physical property | Testing standards | TS-260 | TS-300 | TS-350 |
| Color | Visualization | Gray, Black | Grey, black, Red | |
| Thickness(mm) Tolerance(%) | ASTM D374/D374M / | 1.2~25.4 | 1.2~25.4 ±10 | 1.2~25.4 ±10 |
| Density(kg/m3) | ASTM D1056 | 230 | 270 | 290 |
| Compression-Rebound Stress (kPa,25%) | ASTM D1056 | 10 | 20 | 30 |
| Compression set(%) (Maximum,50%,100℃,22h) | ASTM D1056 | <5 | ||
| Tensile strength (kPa,Minimum) | ASTM D412 | 120 | 150 | 200 |
| Elongation at break(%,Minimum) | ASTM D412 | 50 | 50 | 50 |
| Thermal Conductivity(W/(m·K)) | ASTM E1461 | 0.05 | 0.05 | 0.05 |
| Volume Resistivity(Ω·cm) | ASTM D257 | >1014 | ||
| Flame-retardant Rating | UL 94 | V-0,HF-1 | ||
| UL Yellow Card File Number | / | E499089 | ||
| Recommended operating temperature(℃) | SAE J-2236 | -55~200 | ||
The above data is the average value of the overall test. Please contact our company for more technical information.
Compression rebound curve: